4 MAJOR CAUSES OF GALVANIC CORROSION IN BOILER

GALVANIC CORROSION IN BOILER

Galvanic corrosion occurs by electrical coupling of dissimilar metals or alloys.

CAUSES OF GALVANIC CORROSION IN BOILER

  1. Scratches on the metal surface
  2. Differential stresses in metals
  3. Conductive deposits on boiler surface
  4. Acid cleaning of the boiler



Comments

  1. It is a very informative and useful post thanks it is good material to read this post increases my knowledge. Boiler hire

    ReplyDelete
  2. nice information 4 MAJOR CAUSES OF GALVANIC CORROSION IN BOILER.I like diagrams in this blog
    thanks for sharing
    http://www.maniks.com/manufacturer/air-preheater/

    ReplyDelete
  3. That is sole interesting Giggle My partner and i little girls illuminate vias My business is constantly searching for academic information player this. That is hit what exactly My partner and i was ready for. Blesss pertaining to expressing this huge discourse. That was an interesting hellfire and brimstone to associated with information on screenplay research. Sate expedition numerous with this interesting cook. Ölkessel kaufen

    ReplyDelete

Post a Comment

Popular posts from this blog

Why spirals are provided at the Idustrial Boiler Chimney

Chimney:- Chimney , as we know, is used to reject the flue gases to the atmosphere, coming from the Steam Boiler during operation. Also, it is a megastructure in Steam Boiler assembly and any discrepancy in its structural and foundation work can cause extremely serious damages, may even lead to casualties or plant shut off till its re-erection. The designer must consider all the factors while designing chimneys and one of the major factors amongst them is the wind factor. Blowing wind tries to overcome its static inertia but fails, if spirals are provided on the surface of the chimney. BUT THE QUESTION IS HOW????? Consider a chimneys (without spiral wings) , when the blowing wind comes in contact with its upstream surface, stagnation point (zero velocity) is achieved at that point i.e. pressure generated is high at that point and at the downstream end a vacuum is created as the wind coming in contact with the chimneys , gets deflected and meets after some point (wake regio...

SENSIBLE HEAT & LATENT HEAT

SENSIBLE HEAT Sensible heat produces a rise or fall in temperature of substance Sensible heat does not change physical state of substance LATENT HEAT Latent heat changes the state of substance i.e. Liquid to Gas, Solid to Liquid and Liquid to Solid in case of boiler . Latent heat does not cause temperature change in the substance

Critical Thickness of Insulation and It's Effect on Boiler Efficiency

Welcome to the THERMODYNE BLOG, today in this article we are going to explore the thickness of insulation and its effect on boiler efficiency and other parameters. Critical thickness of insulation and its significance             The information in this article gives a significant collection of data you need to know about the boiler and its performance, the parameter that affects the boiler efficiency .         Table of content INTRODUCTION THICKNESS OF INSULATION CRITICAL RADIUS EFFECT ON BOILER EFFIIENCY INSULATING MATERIALS CONCLUSION INTRODUCTION- The  thickness  up to which heat flow increases and after which heat flow decreases is termed  critical thickness . In the case of cylinders and spheres, it is called the  critical radius . The  critical radius of insulation  can be derived depending on the thermal conductivity of the insulation k and the external convection heat ...